Optimizing bursting behavior of calendered needle-punched polyester fabrics

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 5 publications
(2 citation statements)
references
References 13 publications
0
2
0
Order By: Relevance
“…After hot pressing, the CLN group tends to be softer and exhibits a bursting strength of 736.96 ± 8.60 N. Finally, the NLN group exhibits the lowest bursting strength of 420.65 ± 5.94 N, which is ascribed to the top and bottom layers being nylon spacer fabrics. Nylon spacer fabrics are formed of interconnected loops, and they appear to be sleek, which then compromises the bursting strength of the NLN group [ 38 , 39 , 40 , 41 ].…”
Section: Resultsmentioning
confidence: 99%
“…After hot pressing, the CLN group tends to be softer and exhibits a bursting strength of 736.96 ± 8.60 N. Finally, the NLN group exhibits the lowest bursting strength of 420.65 ± 5.94 N, which is ascribed to the top and bottom layers being nylon spacer fabrics. Nylon spacer fabrics are formed of interconnected loops, and they appear to be sleek, which then compromises the bursting strength of the NLN group [ 38 , 39 , 40 , 41 ].…”
Section: Resultsmentioning
confidence: 99%
“…Certain fibres, such as high-tenacity fibres or fibres with good interlocking properties, can enhance tear resistance when blended appropriately. The fibre blend composition impacts burst strength by influencing the fabric's structural integrity and resistance to internal pressure [5,18,19]. Blending fibres with high tensile strength and good cohesion can improve the burst strength of needle-punched nonwovens.…”
Section: Introductionmentioning
confidence: 99%