Since tungsten (W) has been selected as material for the ITER divertor target the knowledge of the emissivity in the infrared (IR) wavelength range becomes mandatory. A dedicated setup has been developed to measure the emissivity in the wavelength range 1.7-4.75 µm and the temperature domain 200-850 °C. The paper presents the emissivity measurements on W samples coming from actively cooled bulk W components (ITER-like) and W-coated graphite component of the WEST divertor. W samples with damaged surfaces generated by transient heat load as those observed in fusion machines, including micro-cracks and crack network, are also investigated. The dependence on wavelength, temperature and surface state are shown and discussed.