2016
DOI: 10.1557/jmr.2016.141
|View full text |Cite
|
Sign up to set email alerts
|

Oxidation behavior of AISI 321, AISI 316, and AISI 409 stainless steels: Kinetic, thermodynamic, and diffusion studies

Abstract: Abstract

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
6
0
1

Year Published

2017
2017
2024
2024

Publication Types

Select...
7
1
1

Relationship

0
9

Authors

Journals

citations
Cited by 17 publications
(7 citation statements)
references
References 13 publications
0
6
0
1
Order By: Relevance
“…The relatively low surface energy of the composites further confirms their hydrophobic property. Furthermore, the TPU matrix and SS substrate contribute to the weatherability of the SS@TPU/CNT composites, which can ascribe to the antierosion of the TPU polymer and the antioxidation of the SS wire …”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…The relatively low surface energy of the composites further confirms their hydrophobic property. Furthermore, the TPU matrix and SS substrate contribute to the weatherability of the SS@TPU/CNT composites, which can ascribe to the antierosion of the TPU polymer and the antioxidation of the SS wire …”
Section: Resultsmentioning
confidence: 99%
“…Furthermore, the TPU matrix and SS substrate contribute to the weatherability of the SS@TPU/CNT composites, which can ascribe to the antierosion of the TPU polymer 40 and the antioxidation of the SS wire. 41 3.2. Electrical Conductivity of Flexible Conductive SS Warp-Knitted Mesh Fabric and its Composites.…”
Section: Fundamental Properties Of Flexible Conductivementioning
confidence: 99%
“…A Figura 3 (b) mostra o quadrado do ganho de massa da liga estudada, onde é possível observar um incremento linear com o tempo de oxidação, indicando que o comportamento de oxidação dos materiais estudados obedece à lei parabólica. Neste caso, o comportamento de oxidação é controlado por uma difusão iônica, isto é, os íons se difundem através de defeitos pontuais e a espessura da camada de óxido formado corresponde diretamente ao tempo de oxidação (MOVAHEDI-RAD et al, 2016).…”
Section: Resultsunclassified
“…where k p is the parabolic rate constant (kg 2 m −4 s −1 ). The k p value obtained by fitting the experimental data with the least squares method [38,39] is given in Table 5. Weight gain of bare AISI 304 coupon linearly increases with respect to the time and exhibits the highest k p value of 3.5 ± 0.03 × 10 −6 kg 2 m −4 s −1 .…”
Section: Oxidation Kineticsmentioning