Abstract--Iron nI for Ti TM substitution in the structure of pedogenic and synthetic anatase of up to Fe/ (Ti+Fe) 0.1 mol/mol was indicated by an increase in unit cell size as measured by XRD line shifts. MiSssbauer-and electron paramagnetic resonance spectra at both, 298 K and 4.2 K supported this by the presence of signals typical for octahedrally coordinated Fe I11 in a diamagnetic matrix. Charge compensation was achieved by structural OH, as indicated by FTIR bands at 3360 and 960 cm -~, which were absent in pure anatase and which disappeared on heating. The weight loss on heating amounted to ca. 0.5 mol H20/mol Fe. At 600~ structural Fe was ejected, the unit cell size decreased to that of pure anatase, and pseudobrookite, Fe2TiOs, was formed.