“…The effective nanopore radius of the disk, when not varied continuously, was either r p = 1 nm, 10 nm, or 100 nm. The porosity and tortuosity of the nanopores were fixed to = 0.32 and τ = 3.5, respectively, again in consonance with recent experimental reports [31,32] . This resulted in a permeability of k = 1 .…”