Abstract:2223 from 37% to 68%. Based on SEM analysis, the surface area of porosity at the surface of the test object is 4,742%. As for repeated sintering treatment resulted in a decrease of porosity from 4.742% to 2.132% to 1.589% for sintering test 1 times, 2 times, and 3 times. The grain shape is also increasingly more uniform as a result of the repeated sintering treatment given to the sample.
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.