“…8,9,14,27,31,36,57,58,66,[83][84][85][87][88][89][90][91][92] Some authors used the full factorial method for carrying out a suitable number of experiments. 93,94 Related to various researches, many authors 1,2,9,15,20,45,50,53,63,75,77,82,[94][95][96][97][98][99][100][101] discussed the surface morphologies of different materials posterior to SE testing, exhibiting the different mechanism of failure on the observed eroded surface. Surface roughness 'Ra' and 'Rz' are the parameters for characterizing such type of eroded surfaces.…”