“…g 2 is the high aluminum stable phase, a complex cubic structure with stoichiometry Cu 9 Al 4 , coherent with the b matrix [2,3]. It has been recently shown that these alloys, with 23 at% Al, show a hypereutectoid behavior for Be content higher than around 2.9 at%, with g 2 as the first formed phase under slow cooling from high temperature [4]. Their influence on the MT in Cu-based SMA has been extensively studied, mostly in Cu-Zn-Al [5][6][7][8][9], and Cu-Al-Ni alloys [10][11][12].…”