2016
DOI: 10.1016/j.jallcom.2016.02.024
|View full text |Cite
|
Sign up to set email alerts
|

Photocatalytic degradation of malachite green dye using Au/NaNbO3 nanoparticles

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

1
16
0

Year Published

2018
2018
2024
2024

Publication Types

Select...
6
2

Relationship

0
8

Authors

Journals

citations
Cited by 68 publications
(17 citation statements)
references
References 28 publications
1
16
0
Order By: Relevance
“…By extrapolating the linear portion of the Tauc plot to zero, a bandgap value of approximately 3.34 eV is obtained ( Figure 10). is bandgap is comparable to the values of the bandgap of NaNbO 3 reported in the literature, for the nanostructured NaNbO 3 bandgaps produced from Nb 2 O 5 , demonstrating that the initial source does not influence the bandgap obtained [5,8,18]. is bandgap value shows its potential application as a photocatalyst activated in UV range.…”
Section: Advances In Materials Science and Engineeringsupporting
confidence: 82%
See 1 more Smart Citation
“…By extrapolating the linear portion of the Tauc plot to zero, a bandgap value of approximately 3.34 eV is obtained ( Figure 10). is bandgap is comparable to the values of the bandgap of NaNbO 3 reported in the literature, for the nanostructured NaNbO 3 bandgaps produced from Nb 2 O 5 , demonstrating that the initial source does not influence the bandgap obtained [5,8,18]. is bandgap value shows its potential application as a photocatalyst activated in UV range.…”
Section: Advances In Materials Science and Engineeringsupporting
confidence: 82%
“…e hydrothermal synthesis' method has shown promise in manufacturing niobates, both from niobium oxides [1,6,11,12,[16][17][18][19] and from the metallic niobium [4,15].…”
Section: Introductionmentioning
confidence: 99%
“…The rate of decolorization was monitored spectrophotometrically. The effect of different process parameters such as pH (2)(3)(4)(5)(6)(7)(8)(9), initial concentration of dye (5-50 ppm) and amount of catalyst (0.5-1.5 gL -1 ) on degradation of the dye was also observed. It was reported that maximum degradation of dye occurred in acidic range with TiO2 and at neutral pH with ZnO.…”
Section: Introductionmentioning
confidence: 99%
“…Nanocube structure of sodium niobite was prepared by Baeissa [7] using a hydrothermal method. These nanocubes were doped with gold by impregnation with an aqueous solution of HAuCl4.…”
Section: Introductionmentioning
confidence: 99%
“…A literature survey shows that degradation efficiency of CIP has been investigated via HPLC 1 and TLC (Krzek et al, 2005). UV and UV/H2O2 by multiple-wavelength ultraviolet light-emitting diodes (Ou et al, 2016), Photo catalytic synthesized with TiO2 nanoparticles on montmorillonite (Hassani et al, 2015), UV/H2O2 (Baeissa, 2016), photo-Fenton Homogenous (Bobu et al, 2015, Sonolysis (De Bel et al, 2009), and adsorption processes (Jiang et al, 2009). Particularly, Fenton Homogenous processes have been used as one of the best methods to control and reduce organic pollutions, whereby inexpensive and environmentally friendly reagents are employed (Biglarijoo et al, 2016).…”
Section: Introductionmentioning