Photocatalytic TiO2 coatings on limestone

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
31
0
2

Year Published

2014
2014
2024
2024

Publication Types

Select...
5
4
1

Relationship

0
10

Authors

Journals

citations
Cited by 61 publications
(34 citation statements)
references
References 22 publications
1
31
0
2
Order By: Relevance
“…Calcite is its principal constituent, along with very small quantities of clay and other non-carbonate minerals [23,24]. "Lecce stone" has a very high porosity, usually ranging from 30% to 45% [25][26][27], and has a unimodal porosity distribution. In our case, the used samples exhibited a porosity of 42%, with pore sizes mainly between 0.3 and 10 µm, as analysed by mercury-intrusion porosimetry [28].…”
Section: Methodsmentioning
confidence: 99%
“…Calcite is its principal constituent, along with very small quantities of clay and other non-carbonate minerals [23,24]. "Lecce stone" has a very high porosity, usually ranging from 30% to 45% [25][26][27], and has a unimodal porosity distribution. In our case, the used samples exhibited a porosity of 42%, with pore sizes mainly between 0.3 and 10 µm, as analysed by mercury-intrusion porosimetry [28].…”
Section: Methodsmentioning
confidence: 99%
“…From the section analysis the thickness of the coating formed by the aggregation of ultrafine TiO2 can be regarded as falling roughly into the 5-10 μm range (an example of measurement deduced from BSD image is given in Figure 2). The coating was homogeneously spread over stone but its surface was evidently cracked (Figure 2): this outcome may be related to the amount of TiO2 deposited and the subsequent thickness of the coating, over the critical thickness of crack development [29]. It is important to notice by the comparison of the SEM images reported in Figure 2 that cracks were not uniformly present all over the coating but they were present in a punctual manner.…”
Section: Microanalysis Of the Coatingmentioning
confidence: 93%
“…The samples were washed in distilled water, dried in an oven at 105 °C for at least 24 h to reach constant weight. After that, they were left to cool at room temperature and controlled RH 50%, then weighed again [40].…”
Section: Experimental Limestone Specimensmentioning
confidence: 99%