2015
DOI: 10.1016/j.powtec.2014.12.039
|View full text |Cite
|
Sign up to set email alerts
|

Physicomechanical and physicochemical characterizations of biexponential compaction process of paracetamol in the presence of talcum-lubricated-MCC

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
3
0

Year Published

2016
2016
2020
2020

Publication Types

Select...
7
1

Relationship

1
7

Authors

Journals

citations
Cited by 9 publications
(3 citation statements)
references
References 37 publications
0
3
0
Order By: Relevance
“…The pressures which have been used were 0.5,1, 1.5, 2 and 2.5 tons. 14 The dimensions and hardness was then measured for determination of various physical and mechanical properties. 8 Tensile strength was calculated by using formula: 15 Here, F is compression force applied in Newton force (unit: kg.m/S 2 ); d= diameter in meter, h=thickness of the tablet in meter.…”
Section: Direct Compressionmentioning
confidence: 99%
“…The pressures which have been used were 0.5,1, 1.5, 2 and 2.5 tons. 14 The dimensions and hardness was then measured for determination of various physical and mechanical properties. 8 Tensile strength was calculated by using formula: 15 Here, F is compression force applied in Newton force (unit: kg.m/S 2 ); d= diameter in meter, h=thickness of the tablet in meter.…”
Section: Direct Compressionmentioning
confidence: 99%
“…In the coating, talcum powder as a promoter action will be added to the coating which can reduce manufacturing costs and improve the coating hardness [10]. In this paper, the talcum powder was added to waterborne UV curing wood coating, through orthogonal experiment to achieve the composition and curing conditions of process parameters optimization, trying to improve the mechanical properties of waterborne UV curing wood coating and achieve the sub gloss.…”
Section: Introductionmentioning
confidence: 99%
“…Talcum appears inert in most chemical reagents, and does not break down when contacted with acid [20]. Talcum has the low thermal conductivity and high thermal shock resistance, and still not decomposed when heated to 900 • C [21]. The excellent properties of talcum powder make it the good filler and can be used as an additive for coatings.…”
mentioning