2019
DOI: 10.1246/cl.190350
|View full text |Cite
|
Sign up to set email alerts
|

Poly(3,4-ethylenedioxythiophene) Grains Synthesized by Solvent-free Chemical Oxidative Polymerization

Abstract: Poly(3,4-ethylenedioxythiophene) (PEDOT) grains were synthesized by solvent-free chemical oxidative polymerization in one-step and one-pot manner. The resulting PEDOT grains had atypical shapes with a volume-average diameter of 57 ± 45 µm and showed an electrical conductivity of 1.9 × 10−3 S cm−1. Furthermore, it was clarified that the PEDOT grains showed light-to-heat photothermal property.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

1
4
0

Year Published

2019
2019
2022
2022

Publication Types

Select...
5

Relationship

1
4

Authors

Journals

citations
Cited by 5 publications
(5 citation statements)
references
References 22 publications
1
4
0
Order By: Relevance
“…After addition of the monomers to the FeCl 3 powder, an exothermic reaction occurred and temperatures increased to 350, 213, and 190 °C from 25 °C for PPy, PMPy, and PEPy systems, indicating progress of the polymerization. The yields after the purification were gravimetrically determined to be 74% (PPy), 56% (PMPy), and 63% (PEPy), which were similar to those reported previously for P3HT 30 and PEDOT 31 synthesized by solvent-free polymerization (67 and 52%). As comparison, the yields of PPy, PMPy, and PEPy synthesized by aqueous chemical oxidative polymerization were gravimetrically determined to be 89%, 47%, and 2%.…”
Section: Resultssupporting
confidence: 85%
See 2 more Smart Citations
“…After addition of the monomers to the FeCl 3 powder, an exothermic reaction occurred and temperatures increased to 350, 213, and 190 °C from 25 °C for PPy, PMPy, and PEPy systems, indicating progress of the polymerization. The yields after the purification were gravimetrically determined to be 74% (PPy), 56% (PMPy), and 63% (PEPy), which were similar to those reported previously for P3HT 30 and PEDOT 31 synthesized by solvent-free polymerization (67 and 52%). As comparison, the yields of PPy, PMPy, and PEPy synthesized by aqueous chemical oxidative polymerization were gravimetrically determined to be 89%, 47%, and 2%.…”
Section: Resultssupporting
confidence: 85%
“…Solvent-free method: PPy and its derivatives were synthesized as follows, according to method previously reported. , FeCl 3 powder was prepared by grinding pristine powder utilizing a magnetic stirrer bar for 3 min at 750 rpm in a glass vial (200 mL) under N 2 atmosphere. Py or Py derivative monomers (1.5 g: 2.24 × 10 –2 mol (Py), 1.85 × 10 –2 mol (MPy), 1.58 × 10 –2 mol (EPy)) were then added dropwise to the FeCl 3 powder (monomer/FeCl 3 molar ratio, 1/4).…”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…According to the SEM micrographs of all samples in Figure 3 , we can see that the hydrogels’ pore diameters without the addition of PEDOT: PSS are larger compared to the other porous hydrogels. This is due to the viscosity of PEDOT: PSS dispersion, which blocks the pores, causing a reduction in pore sizes [ 53 ]. Physically, this reversed casting method of fabrication created a spongy resistance level in the porous hydrogels.…”
Section: Resultsmentioning
confidence: 99%
“…Conductive PEDOT: PSS solution was prepared using a chemical oxidative polymerization method [ 53 ]. Briefly, 0.05 mL of hydrophobic EDOT was added to 4.50 mL deionized water together with 0.08 mL hydrophilic PSS.…”
Section: Methodsmentioning