Polyimide Aerogels by Ring-Opening Metathesis Polymerization (ROMP)

Abstract: Polyimide aerogel monoliths are prepared by ring-opening metathesis polymerization (ROMP) of a norbornene end-capped diimide, bis-NAD, obtained as the condensation product of nadic anhydride with 4,4 0 -methylenedianiline. The density of the material was varied in the range of 0.13À0.66 g cm À3 by varying the concentration of bis-NAD in the sol. Wet gels experience significant shrinkage, relative to their molds (28%À39% in linear dimensions), but the final aerogels retain high porosities (50%À90% v/v), high su… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

3
84
0

Year Published

2012
2012
2024
2024

Publication Types

Select...
5
4

Relationship

0
9

Authors

Journals

citations
Cited by 140 publications
(87 citation statements)
references
References 69 publications
3
84
0
Order By: Relevance
“…In comparison with some previous reports about polyimide aerogels, the polyimide aerogels showed relatively high shrinkage. 25,30,32 In addition, the shrinkage of the polyimide aerogel increased with increasing the concentration of polyimide containing trimethoxysiloxane side groups in DMF. Shrinkage was reflected upon the bulk densities of the final polyimide aerogels.…”
Section: Scheme 2 Synthesis Route For Cross-linked Polyimide Gel Witmentioning
confidence: 99%
See 1 more Smart Citation
“…In comparison with some previous reports about polyimide aerogels, the polyimide aerogels showed relatively high shrinkage. 25,30,32 In addition, the shrinkage of the polyimide aerogel increased with increasing the concentration of polyimide containing trimethoxysiloxane side groups in DMF. Shrinkage was reflected upon the bulk densities of the final polyimide aerogels.…”
Section: Scheme 2 Synthesis Route For Cross-linked Polyimide Gel Witmentioning
confidence: 99%
“…32 This kind of polyimide aerogel combined facile one-step synthesis with high mechanical strength and specific energy absorption. However, they had unsaturated backbone, which limited their use in air at high temperature.…”
Section: ■ Introductionmentioning
confidence: 99%
“…44 crosslinking process is time-consuming and costly, making the purely organic aerogels more appealing [157]. On the other hand, some industrial applications of aerogels [158] demanded highly flexibility and foldability, which cannot be attainable by the polymer-cross-linked silica aerogels.…”
Section: Accepted Manuscriptmentioning
confidence: 99%
“…Toluene (anhydrous, 99.8%, Aldrich) was purged with nitrogen gas prior to use. Poly(dicyclopentadiene-random-norbornene) (P(DCPD-r-NB) gels were prepared from ring opening metathesis polymerization (ROMP) [46,[53][54][55][56] of DCPD and NB in toluene with Grubbs' 1 st generation catalyst [57]. Density of the P(DCPD-r-NB) aerogels and gelation time were adjusted by the DCPD/NB-to-toluene and the DCPD/NB-to-catalyst ratio, respectively.…”
Section: Uniformity Dependencymentioning
confidence: 99%