Porous Li2FeSiO4/C nanocomposite as the cathode material of lithium-ion batteries

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
102
4

Year Published

2014
2014
2022
2022

Publication Types

Select...
7
1

Relationship

4
4

Authors

Journals

citations
Cited by 178 publications
(110 citation statements)
references
References 31 publications
2
102
4
Order By: Relevance
“…The capacity retention reaches 135 mAh g À1 at rate C/16, and is stable over 40 cycles [222]. Porous Li 2 FeSiO 4 / C nanocomposite with 8.06 wt% carbon showed a capacity of 176.8 mAh g À1 at 0.5C in the first cycle and a reversible capacity of 132 mAh g À1 at 1C (1C ¼ 160 mA g À1 ) in the 50th cycle [223]. If the voltage range extends from 1.5 to 4.8 V, a capacity of 220 mAh g À1 has been reported at low current density 10 mA g À1 , but after three cycles, the capacity was already decreased to circa 190 mAh g À1 [224] [227,228] have been obtained for Li 2 FeSiO 4 annealed at 800 C, while another polymorph has been found upon quenching from 900 C to room temperature [229].…”
Section: Nasicon-like Compoundsmentioning
confidence: 97%
“…The capacity retention reaches 135 mAh g À1 at rate C/16, and is stable over 40 cycles [222]. Porous Li 2 FeSiO 4 / C nanocomposite with 8.06 wt% carbon showed a capacity of 176.8 mAh g À1 at 0.5C in the first cycle and a reversible capacity of 132 mAh g À1 at 1C (1C ¼ 160 mA g À1 ) in the 50th cycle [223]. If the voltage range extends from 1.5 to 4.8 V, a capacity of 220 mAh g À1 has been reported at low current density 10 mA g À1 , but after three cycles, the capacity was already decreased to circa 190 mAh g À1 [224] [227,228] have been obtained for Li 2 FeSiO 4 annealed at 800 C, while another polymorph has been found upon quenching from 900 C to room temperature [229].…”
Section: Nasicon-like Compoundsmentioning
confidence: 97%
“…The crystal structure can be controlled by adjusting the synthetic methods. Generally, the Pmn2 1 phase is prepared by hydrothermal method, and P2 1 /n and Pmnb phase are synthesized via solid state reactions at different tenperatures (600-800°C for P2 1 /n and ≥900°C for Pmnb) [31][32][33][34]. Dominko's group [31] demonstrated that the stronger Fe-O bonds resulted in a lower Fe 2+ /Fe 3+ redox potential.…”
Section: Inorganic Cathode Materialsmentioning
confidence: 99%
“…Therefore, intensive efforts are focused on solving the above mentioned difficulties. According to recent published papers, the effective methods include carbon modification, ion-doping, and nanocrystallization [15,32].…”
Section: Inorganic Cathode Materialsmentioning
confidence: 99%
See 1 more Smart Citation
“…With respect to the first two, some approaches to minimize the particle size and coat the electron-conducting phase using more conductive materials have been carried out and found to be effective in improving both the electronic conductivity and lithium ion diffusion rate of LiFePO 4 [6][7][8][9][10][11][12]. In general, coating electrode materials with carbon could improve the electronic conductivity between particles and provide electronic tunnels.…”