1995
DOI: 10.1016/0008-8846(95)00161-1
|View full text |Cite
|
Sign up to set email alerts
|

Preliminary study of effect of LiNO2 on expansion of mortars subjected to alkali-silica reaction

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
8
0
1

Year Published

1997
1997
2022
2022

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 11 publications
(9 citation statements)
references
References 2 publications
0
8
0
1
Order By: Relevance
“…Later, Stark (Stark, 1992) confirmed the effectiveness of LiF and Li 2 CO 3 in inhibiting ASR expansion, and reported that also LiOH seemed to be effective. Several other studies further reported that also LiBr (Qinghan et al, 1995;Bian et al, 1996;Demir and Arslan, 2013;Demir et al, 2018) and LiH 2 PO 4 (Bian et al, 1996) are effective in reducing ASR expansion. Bian et al (Bian et al, 1996) reported LiCl, LiBr, LiNO 2 , LiNO 3 , Li 2 SO 4 , and LiH 2 PO 4 actually produced similar suppressive effects on ASR expansion, whereas Li 2 CO 3 , LiOH, and LiF only exhibited certain effects at a [Li]/[Na + K] molar ratio of 0.8.…”
Section: Types Of LI Saltsmentioning
confidence: 94%
See 1 more Smart Citation
“…Later, Stark (Stark, 1992) confirmed the effectiveness of LiF and Li 2 CO 3 in inhibiting ASR expansion, and reported that also LiOH seemed to be effective. Several other studies further reported that also LiBr (Qinghan et al, 1995;Bian et al, 1996;Demir and Arslan, 2013;Demir et al, 2018) and LiH 2 PO 4 (Bian et al, 1996) are effective in reducing ASR expansion. Bian et al (Bian et al, 1996) reported LiCl, LiBr, LiNO 2 , LiNO 3 , Li 2 SO 4 , and LiH 2 PO 4 actually produced similar suppressive effects on ASR expansion, whereas Li 2 CO 3 , LiOH, and LiF only exhibited certain effects at a [Li]/[Na + K] molar ratio of 0.8.…”
Section: Types Of LI Saltsmentioning
confidence: 94%
“…In contrast to SCMs, which can only be introduced during concrete production, lithium salt solutions can be applied to an expanding concrete structure in addition to being used as an admixture during production. So far, eleven different types of lithium salts have been studied to mitigate ASR including LiCl, Li 2 CO 3 , LiF, Li 2 SiO 3 , LiNO 3 , Li 2 SO 4 , LiOH, LiNO 2 , LiBr, LiOH•H 2 O, LiH 2 PO 4 (McCoy and Caldwell, 1951;Qinghan et al, 1995;Lumley, 1997;Demir and Arslan, 2013). Some difficulties of using these lithium salts are encountered because the dosage of different types of lithium salts varies significantly depending on several factors such as the type of lithium salts, the mineralogy of reactive aggregates, and the alkali content of the concrete.…”
Section: Introductionmentioning
confidence: 99%
“…The expansion reduction may also be attained by chemical additions to the concrete, like lithium compounds. Qinghan et al [7] and Lumley [8] indicate that lithium compounds are effective to inhibit ASR expansion, because it replaces sodium and potassium alkaline ions in ASR gel, densifying it. Notice that, if insufficient lithium is used, the expansion may increase, because lithium compounds may combine with calcium hydroxide as well, producing calcium salts and lithium hydroxide, and increasing hydroxyl ions concentration in the pore solution [9].…”
Section: Introductionmentioning
confidence: 99%
“…[Li]/[Na] = 0.67-1 (Sakaguchi, 1989) [Li]/[Na+K] > 0.7 (Thomas & Stokes, 1999) [Li]/[Na+K] ≥ 0.92 Stark, 1993) [Li]/[Na+K] > 0.72 (Durand 2000) [Li]/[Na+K] ≥ 0.8 (Collins et al 2004) [Li]/[Na+K] = 0.74 to 0.93 (Fournier et al, 2003) [Li]/[Na+K] ≥ 0.8 (Qinghan et al 1995) [Li]/[Na+K] = 0.56 to 1.11 (Tremblay et al, 2004) Li2CO3 (Note 1): more effective to decrease ASR expansion than LiOH and LiNO3 (Vivian, 1947;Sakaguchi, 1989) [Li]/[Na] = 0.67-1 (Sakaguchi 1989) Li2CO3 = 1.0% by wt. of cement (Ohama et al,.…”
Section: Use Of Chemicals To Prevent Asrmentioning
confidence: 99%