Preparation and characterization of novel bionanocomposite based on soluble soybean polysaccharide and halloysite nanoclay

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

5
30
0

Year Published

2017
2017
2021
2021

Publication Types

Select...
4
2

Relationship

0
6

Authors

Journals

citations
Cited by 74 publications
(35 citation statements)
references
References 35 publications
5
30
0
Order By: Relevance
“…For example, at the strain of 0.22%, the G ′ of CT hydrogel was 39.7 kPa while the CTH4 sample was 125.1 kPa. This means that the incorporation of HNC into the CT matrix remarkably enhanced the stiffness and load bearing capability of the ultimate hydrogels, which is due to the reinforcement effect and restrictions in the chain mobility …”
Section: Resultsmentioning
confidence: 91%
See 3 more Smart Citations
“…For example, at the strain of 0.22%, the G ′ of CT hydrogel was 39.7 kPa while the CTH4 sample was 125.1 kPa. This means that the incorporation of HNC into the CT matrix remarkably enhanced the stiffness and load bearing capability of the ultimate hydrogels, which is due to the reinforcement effect and restrictions in the chain mobility …”
Section: Resultsmentioning
confidence: 91%
“…However, when the amount of HNC was added as 4 wt %, the tensile strength was enhanced up to 0.71 MPa and the elongation at break was reduced to 49.93%. This might be due to the interaction between the hydroxyl groups of CT and HNC seemed to be entrained the rigidity of the structure when the HNC content increased . Thus, the stabilization of the hydrogel composites has been improved at higher nano‐filler loading, resulting in decreased elongation values.…”
Section: Resultsmentioning
confidence: 99%
See 2 more Smart Citations
“…The enhanced interfacial cross-linking of PDA in the system might resulted in a compact structure of the hybrid films and a reduction in the polymer chain mobility, thereby prolonging the pathway of gas molecules and limiting the permeation of water vapor molecules under the dense network [65]. In addition, the water vapor permeation occurred in the empty spaces of polymer amorphous regions rather than the crystalline regions, which might also lead to a reduction in the water vapor passages [66]. This conclusion was consistent with the ATR-FTIR and XRD results.…”
Section: Water Resistance Of Spi-based Hybrid Filmsmentioning