2003
DOI: 10.1016/s0167-577x(02)01409-x
|View full text |Cite
|
Sign up to set email alerts
|

Preparation and characterization of silica-doped titania photocatalyst through sol–gel method

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

7
73
0
1

Year Published

2015
2015
2020
2020

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 148 publications
(89 citation statements)
references
References 18 publications
7
73
0
1
Order By: Relevance
“…The different evidence is happened when the addition of silica into TiO 2 is in a large quantity. Silica can inhibit the formation rutile by impeding direct contact between TiO 2 particle with forming the Ti-O-Si binding [8]. The same phenomenon was also observed on Cr-doped nano-titania in argon [31] where rutile phase is dominant after temperature above 900°C.…”
Section: Photocatalysissupporting
confidence: 56%
See 1 more Smart Citation
“…The different evidence is happened when the addition of silica into TiO 2 is in a large quantity. Silica can inhibit the formation rutile by impeding direct contact between TiO 2 particle with forming the Ti-O-Si binding [8]. The same phenomenon was also observed on Cr-doped nano-titania in argon [31] where rutile phase is dominant after temperature above 900°C.…”
Section: Photocatalysissupporting
confidence: 56%
“…The increasing of photocatalytic activity is shown by the decreasing of sample's absorbance spectrum. On the other hand, silica plays the role as a carrier of titania and enhances the surface area with enough pore size [8]. The modification of titania in enhancing its catalytic properties can also be conducted by adding nitrogen [9], iodine [10], and Cr [11] to titania.…”
Section: Introductionmentioning
confidence: 99%
“…TEOS (Tetraethylorthosilicate) and TTIP (Titanium tetra isopropoxide) were used as precursor. It was observed that the TTIP hydrolysis rate is much faster than TEOS [16]. The synthesis consists of two steps.…”
Section: Tio 2-sio 2 Mixed Oxidementioning
confidence: 99%
“…To assess the durability of the SiO 2 , TiO 2 and SiO 2 @TiO 2 coated samples, an adherence test was performed following the ASTM 3359 [21] and the appropriate references [22][23][24][25][26][27]. In this case, the corresponding test for thin films with thicknesses less than or equal to 2 mm was selected.…”
Section: Durabilitymentioning
confidence: 99%
“…Then, the scotch tape was removed from the opposite end of the application, forming a 180 • angle. Next, the coated area was compared with the patterns presented in Table 2 [22][23][24][25]. In addition, the adherence test was carried out before and after UV light exposure (0, 4 and 26 h), to determine the photocatalytic activity of the SiO 2 @TiO 2 coating.…”
Section: Durabilitymentioning