“…Compared with blank paper sheet, whose surface strength and smoothness are 0.69 m s -1 and 37.6 s, the surface strength of paper sheets treated with 0.2, 0.4, 0.6, and 0.8 wt% of PFBD, respectively, increase by 0.76, 1.15, 1.51, and 1.84 m s -1 . Meanwhile, the smoothness of surface-sized paper sheets, respectively, boosts by 45.5, 50.9, 54.1, and 56.7 s. Therefore, with the increase concentration of PFBD, the surface strength and smoothness of paper sheets are heightened, which indicates that PFBD has good film-forming property, which can be applied in the paper industry as a surface-sizing agent [34,35] (the coating weights of PFBD are 0.1, 0.2, 0.3, and 0.4 g m -2 , while the dosages of PFBD are 0.2, 0.4, 0.6, and 0.8 wt%).…”