Preparation, characteristics and corrosion properties of α-Al2O3 coatings on 10B21 carbon steel by micro-arc oxidation

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
8
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 19 publications
(8 citation statements)
references
References 16 publications
0
8
0
Order By: Relevance
“…At the same time, plasma electrolysis of carbon steel with added α-Al 2 O 3 in the electrolytic bath generated coatings with improved corrosion behavior [19]. Additionally, α-Al 2 O 3 -based coatings on carbon steel substrate prepared by plasma electrolytic oxidation increased the protection against wear and corrosion conditions [20].…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…At the same time, plasma electrolysis of carbon steel with added α-Al 2 O 3 in the electrolytic bath generated coatings with improved corrosion behavior [19]. Additionally, α-Al 2 O 3 -based coatings on carbon steel substrate prepared by plasma electrolytic oxidation increased the protection against wear and corrosion conditions [20].…”
Section: Introductionmentioning
confidence: 99%
“…In this regard, aluminum and aluminum-titanium oxide layers have been successfully prepared on pure Ti when surface hardening and corrosion protection was required [15,16]. Similarly, another approach is to develop and maximize α-Al 2 O 3 within the coatings with the aim of enhancing mechanical and corrosion properties of various alloys [17][18][19][20]. Ghafaripoor [17] reported that an increase of corrosion and tribocorrosion resistance occurred after PEO processing the Al alloy substrate in an electrolyte containing α-Al 2 O 3 particles.…”
Section: Introductionmentioning
confidence: 99%
“…This increases the rate of material removal by causing continuous delamination to occur on the surface of the specimen up until it begins to pull off from the pin surface (figure 11(b)). At longer sliding distances (1500 m), small amounts of delamination and wear debris are seen for TiC coating, primarily as a result of MML development on the surface of pin (figure 11(c)), a corresponding decline in the rate of material wear is seen in these circumstances [58]. Through continuous sliding, the dislocations occur on the surface at a certain distance.…”
Section: Worn Surface Analysismentioning
confidence: 99%
“…α-Al 2 O 3 is a high-temperature stable form of Al 2 O 3 , which is one of the important structural materials because of its low cost, low thermal conductivity, high hardness, high flexure strength, high dielectric strength, excellent chemical inertness, high wear resistance, and corrosion resistance. [1][2][3] These excellent properties make Al 2 O 3 coating have a high potential for broad applications in wear, corrosion, and dielectric protections. Atmospheric plasma spraying (APS) processes are performed at atmospheric pressure with high input power and plasma flame temperatures.…”
Section: Introductionmentioning