2006
DOI: 10.2497/jjspm.53.769
|View full text |Cite
|
Sign up to set email alerts
|

Processing of Net-shaped Fe-Ni Nanomaterials by Powder Injection Molding

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2012
2012
2014
2014

Publication Types

Select...
2
1

Relationship

0
3

Authors

Journals

citations
Cited by 3 publications
(1 citation statement)
references
References 15 publications
0
1
0
Order By: Relevance
“…Figure 13 shows the shape and surface roughness of the PIM gear of Fe–8 wt % Ni wet-milled powder after debinding and sintering (sintered at 1000 °C for 1 h) [5,21,26]. As clearly seen, the PIM part keeps its fine gear-shape with uniform full density and no distortion.…”
Section: Application Of Nas To Fabrication Of Iron Base Powder Matmentioning
confidence: 99%
“…Figure 13 shows the shape and surface roughness of the PIM gear of Fe–8 wt % Ni wet-milled powder after debinding and sintering (sintered at 1000 °C for 1 h) [5,21,26]. As clearly seen, the PIM part keeps its fine gear-shape with uniform full density and no distortion.…”
Section: Application Of Nas To Fabrication Of Iron Base Powder Matmentioning
confidence: 99%