2012
DOI: 10.1016/j.conbuildmat.2012.04.044
|View full text |Cite
|
Sign up to set email alerts
|

Production of geopolymeric binder from blended waste concrete powder and fly ash

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

7
89
1
1

Year Published

2014
2014
2024
2024

Publication Types

Select...
6
2
1

Relationship

0
9

Authors

Journals

citations
Cited by 300 publications
(98 citation statements)
references
References 48 publications
7
89
1
1
Order By: Relevance
“…This can be ascribed to the formation of a geopolymer gel created during dissolution of the FA glassy phase [28]. It is notable that the quartz and mullite peaks were still present but with reduced intensity, after NaOH activation.…”
Section: X-ray Diffraction (Xrd)mentioning
confidence: 98%
“…This can be ascribed to the formation of a geopolymer gel created during dissolution of the FA glassy phase [28]. It is notable that the quartz and mullite peaks were still present but with reduced intensity, after NaOH activation.…”
Section: X-ray Diffraction (Xrd)mentioning
confidence: 98%
“…Increased water absorption with the increased pressure causes higher amounts of NaOH solution is squeezed out [17]. In such conditions, the geopolymerization reaction blocked so geopolymer gel formed slightly and then produce a high porosity of the geopolymer matrix.…”
Section: B Effect Of Si/al Ratio To Water Absorptionmentioning
confidence: 99%
“…A Philips XL30 ESEM-TMP FEI scanning electron microscope was used for an identification of individual phases and their levels at 100× magnification. A scanning electron microscopy (SEM) was used in BSE (backscattered electrons) mode at a low pressure (10)(11)(12)(13)(14)(15)(16)(17)(18)(19)(20) and at an accelerating voltage of 30 kV. Figure 1 illustrates the heat evolution.…”
Section: Measurement Methodsmentioning
confidence: 99%
“…Ahmari et al [19] developed a geopolymer based binder using the RCP, together with fly ash. As a source of silicon and calcium, the RCP, at a maximum quantity of 50 wt%, contributes to a solid bond between the new aggregate and the binder, resulting in a greater compressive strength of the geopolymer, which is in the form of a poly-sialate-disiloxo, and therefore forms a stronger bond than a geopolymer created using fly ash alone.…”
Section: The Rcb As a Bindermentioning
confidence: 99%