1.4 • 1015 to 5.38 • 10 ~1 s cm at 200~ with increase in Na § concentration.Figure 4 shows the variation in conductivity as a function of reciprocal temperature. Two distinct regions were observed. The activation energy was calculated from these plots. The activation energy decreases with increase in Na § concentration from 0.37 to 0.2 eV at low temperature and 1.32 to 0.91 eV at higher temperature regions.Dielectric parameters (e and tan 8) were measured from 102-106 Hz at 25 ~ 100 ~ and 200~ A decrease in dielectric constant was observed with increase in frequency (Fig. 5 and 6). Dependence of dielectric loss on temperature and frequency is shown in Fig. 7 and 8. By the addition of Na § loss value increased from 0.16 to 0.8.
Conclusions1. Cyclodehydration of poly(amide-acid) is influenced by the presence of Na + ions. An increase in Na + ion concentration resulted in a decrease in cyclodehydration reaction.2. The conductivity measurement showed sodium ion participation in conduction.3. A decrease in resistivity and activation energy is observed with increase of sodium ion concentration.