1995
DOI: 10.1299/kikaic.61.3762
|View full text |Cite
|
Sign up to set email alerts
|

Quick Evaluation of Thermal Contact Resistance in Hot and Warm Forging.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3

Citation Types

0
3
0

Year Published

2006
2006
2017
2017

Publication Types

Select...
3

Relationship

2
1

Authors

Journals

citations
Cited by 3 publications
(3 citation statements)
references
References 0 publications
0
3
0
Order By: Relevance
“…Compared with casting forming, the forging can eliminate the defects of the casting state caused by the metal in smelting process, and optimize the microstructure of the metal, and also can improve the mechanical properties of the parts by keeping the integrity of the metal flow line [7][8][9][10][11]. So, the important parts, which are high load and hard working condition, are generally made in the forging method.…”
Section: Introductionmentioning
confidence: 99%
“…Compared with casting forming, the forging can eliminate the defects of the casting state caused by the metal in smelting process, and optimize the microstructure of the metal, and also can improve the mechanical properties of the parts by keeping the integrity of the metal flow line [7][8][9][10][11]. So, the important parts, which are high load and hard working condition, are generally made in the forging method.…”
Section: Introductionmentioning
confidence: 99%
“…In order to improve the die life, to increase the accuracy of the forged products and to reduce forging cost, the heat flux should be controlled. The most significant factor governing heat transfer is the contact condition between the workpiece and die [6]. The contact conditions can be varied by lubricants, tool surface finishing and tool surface modification and so on.…”
Section: Introductionmentioning
confidence: 99%
“…These simulation techniques for die design have been introduced even into medium-and small-sized forging companies in Japan. For dies used in hot forging, die life is affected largely by thermal load; therefore, temperature, thermal deterioration and thermal softening of dies should be estimated [1][2][3][4][5][6][7][8][9][10][11][12][13][14]. Although significant changes in the temperature field of dies occur at the initial stage of forging or at the restart after a pause during forging, the temperature gradually achieves a steady thermal cycle after 20-30 shots.…”