“…Most efforts have been made on improvement of anti-sintering and -coke Ni-based catalyst, for instance, by adding promoters (alkali, alkali earth, and rare earth metal oxides) or/and utilizing different supports (Al 2 O 3 , ZrO 2 , SiO 2 , La 2 O 3 and Y 2 O 3 ) [8][9][10][11]. The formation of 'hotspots' in the catalyst bed is considered as the one of the main causes for the Ni-sintering and carbon deposition [12]. Thus, to develop a novel catalyst system combining excellent catalytic performance with enhanced heat transfer is a promising strategy to overcome these major drawbacks.…”