“…[217,218,221] In the case of wet processing, old magnets are first crushed and ground, before mineral acids dissolve the resulting magnet powder completely.I ng eneral, hydrochloric acid, [217,218,227] nitric acid, [225] sulfuric acid, [225,228] or acetic acid are used for leaching. Mixing 30 wt %EoL magnet powder with 70 wt %ofthe starting alloys resulted in remanence loses of only 3%,which was enough to already miss the high standards.…”