Research on interface characteristics of 308L stainless steel coatings manufactured by laser hot wire cladding

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
6
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 14 publications
(6 citation statements)
references
References 45 publications
0
6
0
Order By: Relevance
“…During solidification, δ-ferrite is the starting phase and follows austenitic transformation by a peritectic-eutectic reaction. 14 Most of the ferrite is transformed into austenite and a small fraction of ferrite is retained due to constitutional supercooling. The transformation of ferrite to austenite will happen till the temperature decreases and until preventing the elemental diffusion.…”
Section: Resultsmentioning
confidence: 99%
See 3 more Smart Citations
“…During solidification, δ-ferrite is the starting phase and follows austenitic transformation by a peritectic-eutectic reaction. 14 Most of the ferrite is transformed into austenite and a small fraction of ferrite is retained due to constitutional supercooling. The transformation of ferrite to austenite will happen till the temperature decreases and until preventing the elemental diffusion.…”
Section: Resultsmentioning
confidence: 99%
“…Multi-layer weld overlaying leads to complex cyclic thermal history influencing the microstructure and mechanical features. 14,15 According to the existing literature, various studies have been made on the CR of Ni-Cr-Mo coatings and the various steel welds in salt environments. [16][17][18] Based on the mentioned literature, the research attempts emphasized the multilayer deposition of stainless steels, Ni-based superalloys as a coating material, and the influence of alloying elements on the microstructure and mechanical properties.…”
Section: Introductionmentioning
confidence: 99%
See 2 more Smart Citations
“…Finally, by reducing the bead width while increasing the bead height, a more rounded ball-shaped bead is formed (Figure 5d). The calculation method for dilution rate is shown in Figure 5e [28]. applications.…”
Section: Single-pass Single-layer Welding Seam Formation Testmentioning
confidence: 99%