Research Status of Graphene Polyurethane Composite Coating

Abstract: Graphene material has a variety of excellent properties and applications in energy storage, biomaterials, photoelectric devices, and other fields. With the progress of nanotechnology, graphene nanomaterials have shown their advantages in the field of new nano-corrosion coatings with their high barrier structure. In addition, polyurethane is also widely used in the field of anti-corrosion coatings due to its excellent chemical resistance, mechanical properties, and weathering resistance. The preparation of comp… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
5
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 8 publications
(5 citation statements)
references
References 53 publications
0
5
0
Order By: Relevance
“…The sand ability and alkali resistance of the paint films show no significant difference, displaying the same performance levels. [39,40]. However, the water resistance and alcohol resistance of the composite coating exhibit promotion as the added GO is not lower than 0.1wt%.…”
Section: Resultsmentioning
confidence: 98%
“…The sand ability and alkali resistance of the paint films show no significant difference, displaying the same performance levels. [39,40]. However, the water resistance and alcohol resistance of the composite coating exhibit promotion as the added GO is not lower than 0.1wt%.…”
Section: Resultsmentioning
confidence: 98%
“…Therefore, at CF, the adhesive area of the strips was stronger than the cross-sectional area of the strip. This indicates a high adhesion of the fiber with the PU, suggesting a good interaction of the matrix-fiber interface [ 44 ]. On the other hand, AF achieved the lowest adhesion performance (0.43 MPa), possibly due to the high basis weight, which prevents the PU adhesive from penetrating all the fibers and permeating the entire fabric.…”
Section: Resultsmentioning
confidence: 99%
“…At the same time, the cross-section became rougher with the increasing GO concentration. This might be caused by the polar groups of GO leading to agglomeration and the appearance of defects [ 47 ]. Moreover, for the same reason, the glossiness of the WPU-GO coatings showed a gradual decrease with increasing GO concentration ( Figure S2 ).…”
Section: Resultsmentioning
confidence: 99%