“…In general, reasonably good catalyst activity was observed under milder reaction conditions compared to previously reported recycling systems. 14,15,18,33,37,38,43,[65][66][67][68][69] In all instances, an increase in temperature coincided with higher Me-LA yield (Y Me-LA ) and shorter reaction times, consistent with the literature. 35,41,43 Zn(2) 2 exhibited superior activity compared to Zn(1,3) 2 at 50°C, suggesting inductive effects dominate, whilst Zn(1) 2 exhibited the lowest degradation activity, both consistent with polymerisation results (Table 3).…”