Selective deposition of chemically-bonded gold electrodes onto PDMS microchannel side walls

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

0
10
0

Year Published

2017
2017
2023
2023

Publication Types

Select...
6
2

Relationship

0
8

Authors

Journals

citations
Cited by 14 publications
(10 citation statements)
references
References 30 publications
0
10
0
Order By: Relevance
“…A suspension of powdered CB (50 nm particle size, Vulcan XC 72 Cabot Corporation) was mixed with PDMS (Sylgard 184, Corning Inc.) in a five-step process modified from previously reported works: (i) CB was suspended in hexane in a 1:10 (w/w) ratio and sonicated at 220 W for 10 min. (ii) Base elastomer was also dissolved in hexane in a 1:2 (w/w) ratio in a different container.…”
Section: Experimental Methodsmentioning
confidence: 99%
“…A suspension of powdered CB (50 nm particle size, Vulcan XC 72 Cabot Corporation) was mixed with PDMS (Sylgard 184, Corning Inc.) in a five-step process modified from previously reported works: (i) CB was suspended in hexane in a 1:10 (w/w) ratio and sonicated at 220 W for 10 min. (ii) Base elastomer was also dissolved in hexane in a 1:2 (w/w) ratio in a different container.…”
Section: Experimental Methodsmentioning
confidence: 99%
“…Preparation of CB-PDMS composite. A suspension of powdered CB (50-nm particle size, Vulcan XC 72 Cabot Corporation), was mixed with PDMS (Sylgard 184, Corning Inc.) in a five step process modified from previously reported works [51][52][53] : i) CB was suspended in hexane in a 1:10 (w/w) ratio and sonicated at 220 W for 10 min. ii) Base elastomer was also dissolved in hexane in a 1:2 (w/w) ratio in a different container.…”
Section: Experimental Methodsmentioning
confidence: 99%
“…Preparation of CB-PDMS composite. A suspension of powdered CB (50-nm particle size, Vulcan XC 72 Cabot Corporation), was mixed with PDMS (Sylgard 184, Corning Inc.) in a five step process modified from previously reported works [58][59][60] : i) CB was suspended in hexane in a 1:10 (w/w) ratio and sonicated at 220 W for 10 min. ii) Base elastomer was also dissolved in hexane in a 1:2 (w/w) ratio in a different container.…”
Section: Experimental Methodsmentioning
confidence: 99%