“…The areal hole density is 8.82 × 10 13 cm −2 , close to that for MoO 3 -doped diamond (4.7 × 10 13 and 6 × 10 13 cm −2 in theoretical results, [22,23] and 2.7 × 10 13 , 1.9 × 10 13 , and 1 × 10 14 cm −2 in experimental results [15,22,24] ), CrO 3 -doped diamond (9.85 × 10 13 cm −2 ), [16] and V 2 O 5 -doped diamond (2.17 × 10 13 and 7 × 10 13 cm −2 ). [17,23] The DOS is further calculated by HSE06 functional in Figure S5 (Supporting Information), the spin-polarization is not considered due to the longer computer time for HSE06 functional. The p-type surface conductivity is also found, and the areal hole density is 5.42 × 10 13 cm −2 , denoting the reliability of PBE calculations.…”