2009
DOI: 10.1016/j.ssi.2009.10.009
|View full text |Cite
|
Sign up to set email alerts
|

Sintering kinetics and oxide ion conduction in Sr-doped apatite-type lanthanum silicates, La9Sr1Si6O26.5

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

5
9
0
2

Year Published

2011
2011
2023
2023

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 19 publications
(16 citation statements)
references
References 23 publications
5
9
0
2
Order By: Relevance
“…Shaula et al 23 reported a total conductivity value of 3 × 10 −2 S cm −1 at 700 • C for pellets with the same composition (92%TD) using a dry reaction sintering methodology applying a final synthesis-sintering step of 1650 • C/10 h. At temperatures below 800 • C, M-34-U2-10BP tape shows higher conductivity values than YSZ. Similar conductivity values were reported by Bonhomme et al 16 for a thick monolithic electrolyte sample prepared by laminated stacks from oxy-apatite powders (La 9 SrSi 6 O 26.5 ). …”
Section: Resultssupporting
confidence: 88%
See 1 more Smart Citation
“…Shaula et al 23 reported a total conductivity value of 3 × 10 −2 S cm −1 at 700 • C for pellets with the same composition (92%TD) using a dry reaction sintering methodology applying a final synthesis-sintering step of 1650 • C/10 h. At temperatures below 800 • C, M-34-U2-10BP tape shows higher conductivity values than YSZ. Similar conductivity values were reported by Bonhomme et al 16 for a thick monolithic electrolyte sample prepared by laminated stacks from oxy-apatite powders (La 9 SrSi 6 O 26.5 ). …”
Section: Resultssupporting
confidence: 88%
“…In this way, oxy-apatite tapes and coatings have been recently prepared by tape casting, [15][16][17] plasma spraying 18 and sputtering. 19 Tape casting is a low-cost well established technique for manufacturing self-supporting ceramic sheets with a wide range of thicknesses (50-500 m) in a continuous way, and has been generally used for the fabrication of microelectronic components.…”
Section: Introductionmentioning
confidence: 99%
“…and the treatment at 1400°C led to the excessive precipitation of the lanthanum‐rich secondary phase from the grain surface of samples with x = +0.5. Similar behavior was reported for Sr‐doped apatite‐type lanthanum silicates: below 1450°C a secondary phase exists and above 1500°C a clean boundary was shown by TEM . On the other hand, the surface of the samples with x = 0 and −0.25 is shown to be clean.…”
Section: Resultssupporting
confidence: 81%
“…Mg, Sr, Ba as alkaline earth metal [7,9,10] are widely used to substitute the La position, and Sr is the most common element [11,12] due to its similar chemical properties with La. As an example of Sr substitution is the Sr-doped apatite-type lanthanum silicates (La 9 Sr 1 Si 6 O 26.5 ) synthesized by Bonhomme et al [13]. A large number of works are also focused on the Si position doping.…”
Section: Introductionmentioning
confidence: 99%
“…(La 10Àx Sr x (Si,Ge) 6 in the table represents La 10Àx Sr x (Si,Ge) 6 O 27À0.5x for short, similarly hereinafter.) (La 10 Sr 0 )Ge 6 [14] (La 10 Sr 0 )Si 6 [8,30] (La 9 Sr 1 )Si 6 [13] (La 8 Sr 2 )Si 6 [8,30] Ionic conductivity (S cm À1 , 700°C) …”