SAE Technical Paper Series 1983
DOI: 10.4271/830632
|View full text |Cite
|
Sign up to set email alerts
|

Softening in Weld Heat Affected Zone of Dual Phase Steel Sheet for Automotive Wheel Rim

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
5
0

Year Published

2006
2006
2021
2021

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 14 publications
(5 citation statements)
references
References 0 publications
0
5
0
Order By: Relevance
“…Heat affected zone softening during welding of DP780 and DP980 spot welds has been reported in the literature. 19,20,70,[115][116][117][118][119][120][121][122][123][124][125] The location of HAZ softening corresponds to the subcritical HAZ. Figure 16 shows microstructure of subcritical HAZ in DP980 spot welds, indicating a tempered martensite microstructure.…”
Section: Heat Affected Zone Softening In Dp Steelsmentioning
confidence: 99%
“…Heat affected zone softening during welding of DP780 and DP980 spot welds has been reported in the literature. 19,20,70,[115][116][117][118][119][120][121][122][123][124][125] The location of HAZ softening corresponds to the subcritical HAZ. Figure 16 shows microstructure of subcritical HAZ in DP980 spot welds, indicating a tempered martensite microstructure.…”
Section: Heat Affected Zone Softening In Dp Steelsmentioning
confidence: 99%
“…The first two factors are influenced by welding process parameters and governed by the net heat input and power density distribution. Previous studies on the weldability of DP 600 indicated that a reduction in strength occurred due to softening in the heat-affected zone [5].…”
Section: Introductionmentioning
confidence: 94%
“…Heat affected zone softening during welding of DP steels has been reported in the literature. 2,4,7,20,[25][26][27][28] The location of HAZ softening corresponds to the subcritical HAZ (i.e. the region in HAZ which experiences temperatures below A c1 critical 2 Effect of welding current and welding time t on FZ size and failure mode: arrows show critical FZ size for each grade below which IF (or partial interfacial) mode was obtained and above that PF mode was observed temperature).…”
Section: Factors Controlling Failure Mode Of Dp Rswsmentioning
confidence: 99%
“…Heat affected zone softening during welding of DP steels has been reported in the literature. 2,4,7,20,[25][26][27][28] The location of HAZ softening corresponds to the subcritical HAZ (i.e. the region in HAZ which experiences temperatures below A c1 critical temperature).…”
Section: Factors Controlling Failure Mode Of Dp Rswsmentioning
confidence: 99%