“…When ZnO NPs was loaded at 1 wt %, 5 wt %, and 10 wt %, the CTE value were reduced to 33.5 ppm/K, 31.3 ppm/K, and 30.1 ppm/K, respectively. Moreover, the TMA thermograms of the ZSQ showed no discernible transitions, which indicated that the nanosized ZnO NPs were well dispersed and the photocuring process complete . In addition, the nanoindentation results of UV‐cured LPMSQ, as well of ZnO composites, were summarized in Figure (B) As shown, both the modulus and hardness values drastically increased with increasing ZnO content.…”