Stress Corrosion Cracking Behavior of 20MnTiB High-Strength Bolts in Simulation of Humid Climate in Chongqing

Abstract: 20MnTiB steel is the most widely used high-strength bolt material for steel structure bridges in China, and its performance is of great significance to the safe operation of bridges. Based on the investigation of the atmospheric environment in Chongqing in recent years, the corrosion solution to simulate the humid climate of Chongqing was designed in this study, and the stress corrosion experiment of high-strength bolts in the simulated humid climate of Chongqing was carried out. The effects of temperature, pH… Show more

Help me understand this report
View published versions

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Publication Types

Select...

Relationship

0
0

Authors

Journals

citations
Cited by 0 publications
references
References 4 publications
0
0
0
Order By: Relevance

No citations

Set email alert for when this publication receives citations?