2021
DOI: 10.1016/j.enmm.2021.100581
|View full text |Cite
|
Sign up to set email alerts
|

Structural and optical properties of MgNb2O6 NPs: Its potential application in photocatalytic and pharmaceutical industries as sensor

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
6
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 20 publications
(7 citation statements)
references
References 43 publications
0
6
0
Order By: Relevance
“…All the Bragg's reflections at (011), (101), (111), ( 200), (021), (022), (112), ( 221), ( 131) and (311) of the host ZrO 2 nanoparticles were in compliance with the data associated with the JCPDS Card No: 37-1484 and were well matched with the monoclinic phases of the synthesized MZNPs. 18 The nature of the peak patterns confirmed the crystallinity and monoclinic-type structure of the MZNPs. The average particle size of the synthesized MZNPs was found to be in the range of 25-38 nm using Scherrer's formula (eqn (1)).…”
Section: Pxrd Analysismentioning
confidence: 66%
“…All the Bragg's reflections at (011), (101), (111), ( 200), (021), (022), (112), ( 221), ( 131) and (311) of the host ZrO 2 nanoparticles were in compliance with the data associated with the JCPDS Card No: 37-1484 and were well matched with the monoclinic phases of the synthesized MZNPs. 18 The nature of the peak patterns confirmed the crystallinity and monoclinic-type structure of the MZNPs. The average particle size of the synthesized MZNPs was found to be in the range of 25-38 nm using Scherrer's formula (eqn (1)).…”
Section: Pxrd Analysismentioning
confidence: 66%
“…This degradation experiment was conducted within a glass reactor, where 20 mg of the catalyst was meticulously added to solutions containing 20 ppm of AR-88. [33,34] Subsequently, the reaction mixture was subjected to UV light irradiation, employing a 125 W pressure Hg lamp. To monitor the progress of the degradation process, aliquots of 5 mL were systematically extracted at 15-minute intervals during the reaction, with a maximum reaction time of 120 min for analysis.…”
Section: Resultsmentioning
confidence: 99%
“…In the photocatalytic dye decoloration reaction, the water and oxygen molecules are directly influencing the formation of superoxide radicals (O 2 •– ) by the presence of e – in the conduction band (eq ) and hydroxyl radicals (OH •– ) (eq ) by the presence of holes in the valence band, respectively. The generated radicals play a vital role in the photocatalytic dye decoloration activities by braking of complex dye structures into eco-friendly byproducts. , normalA normalg ( C u O C u 2 O ) normalC normalu + normalh ν ( l i g h t e n e r g y ) normalA normalg ( C u O C u 2 O ) normalC normalu * ( e n e r g y ) normalA normalg false( normalC normalu normalO normalC normalu 2 normalO false) normalC normalu * ( e n e r g y ) .25em normalA …”
Section: Photocatalytic Studies Of C3 and C3ag5 Nanocompositesmentioning
confidence: 99%
“…The generated radicals play a vital role in the photocatalytic dye decoloration activities by braking of complex dye structures into eco-friendly byproducts. 44 , 45 …”
Section: Photocatalytic Studies Of C3 and C3ag5 Nanocompositesmentioning
confidence: 99%
See 1 more Smart Citation