“…A prior investigation revealed that SDF's specific surface area was crucial to both its physicochemical and functional characteristics ( Zhang et al, 2023 ). After SE treatment, the particular surface region of SDF rose 2.93 times, from 73.3 m 2 /kg (that of O-SDF) to 214.6 m 2 /kg (that of SE-SDF).…”