“…Other researchers have found that pre-sulfiding the Mo catalyst prior to HDS can lead to a more active catalyst than allowing it to gain sulfur in situ [27][28][29]. To this end, the substrates were exposed to an H 2 S/H 2 mixture (25% H 2 S in H 2 ) for 1 h at 200°C in the quartz reaction tube just prior to HDS.…”