Study on Interaction Mechanism of Different Atomic Ratio of Neodymium, Arsenic and Iron

Abstract: In this study, neodymium and arsenic were sealed into industrial pure iron cylinders at a temperature of 1223 K for 50 h. The interaction mechanism of the Nd-Fe-As system at various atomic ratios was investigated by optical microscopy, X-ray diffractometry, and scanning electron microscopy. Binary compounds Fe12As5, NdAs, Fe2As, and Fe17Na2 were the main products formed, with traces of NdFeAs compounds. In addition, at high temperatures, As content affected the diffusion of Fe atoms; the diffusion of Fe increa… Show more

Help me understand this report
View published versions

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Publication Types

Select...

Relationship

0
0

Authors

Journals

citations
Cited by 0 publications
references
References 13 publications
0
0
0
Order By: Relevance

No citations

Set email alert for when this publication receives citations?