Sub-nL thin-film differential scanning calorimetry chip for rapid thermal analysis of liquid samples

Abstract: Differential scanning calorimetry (DSC) is a popular thermal analysis technique. The miniaturization of DSC on chip as thin-film DSC (tfDSC) has been pioneered for the analysis of ultrathin polymer films...