“…[N 2222 ][Gly] and [HDBU][Im] were prepared via one step method as our previous work. , The fluid porous IL composites with different emulsifiers (H-15, H-18, H-20, H-20RH, and H-2000), different emulsifier contents (0.67, 1.33, 2.00, 2.67, and 3.33 wt %), different shear times (1, 2, and 3 min) and rates (10,000, 15,000, and 20,000 rpm) used in this experiment were prepared via same process based on the Pickering emulsion method . Taking AAIL-H20-IL 1 /IL 2 -98% as an example, 2.0 wt % hydrophobic silica (H-20) was added into mixtures of 50 wt %[Emim][Tf 2 N] and 50 wt % [HDBU][Im] (2 mL) in a plastic container.…”