“…The diffraction patterns by XRD of the pristine cotton, GO, and rGO deposited cotton fabric surfaces are displayed in Figure 3d, the diffraction spectra of cotton, GO‐cotton, and rGO‐cotton have typical diffraction peaks of cotton pattern, which exhibit four characteristic peaks at 2θ value of 15° (101), 16.6° (), 22.9° (002), and 34.7° (040), corresponding to monoclinic cellulose‐Iβ (C 6 H 10 O 5 ) n . [ 38 ] Comparison of the three curves shown in Figure 3d shows no characteristic peak of GO and rGO from the diffraction measurements. It is thus difficult to find the characteristic peak of GO and rGO in the pattern of the modified cotton fabric samples, which are at the 2θ values of 10 and 22°, respectively.…”