Suspension Characteristics and Electrophoretic Deposition ofp-Type Bi2Te3Films for Thermoelectric Applications

Abstract: Suspension characteristics and electrophoretic deposition of p-Type Bi2Te3 films for thermoelectric applications

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
5
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
4
1

Relationship

2
3

Authors

Journals

citations
Cited by 5 publications
(5 citation statements)
references
References 62 publications
0
5
0
Order By: Relevance
“…To prepare Bi2Te3 films, the time and voltage of the EPD process were 100V and 10 minutes, respectively. More details about the starting powder, the EPD process and film preparations have been reported elsewhere [21,22]. The media of the EPD suspensions were 100% vol.…”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…To prepare Bi2Te3 films, the time and voltage of the EPD process were 100V and 10 minutes, respectively. More details about the starting powder, the EPD process and film preparations have been reported elsewhere [21,22]. The media of the EPD suspensions were 100% vol.…”
Section: Methodsmentioning
confidence: 99%
“…; it has also been utilized for various medical and industrial applications, such as corrosion protection, for many years [13]. However, a limited amount of research has been reported on various TE materials such as Bi2Te3, which is the focus component of this investigation [19][20][21][22][23].…”
Section: Introductionmentioning
confidence: 99%
“…To prepare Bi2Te3 films, the time and voltage of the EPD process were 100V and 10 minutes, respectively. The details of the starting powder, the EPD process and film preparations have been reported elsewhere [18,19]. The media of the EPD suspensions were 100% vol.…”
Section: Methodsmentioning
confidence: 99%
“…; it has also been utilized for various medical and industrial applications, such as corrosion protection, for many years [10]. However, a very limited amount of research has been reported on various TE materials such as Bi2Te3, which is the focus component of this investigation [16][17][18][19]. This article reports on fabrication of crack-free uniform microstructures of n-type Bi2Te3 films deposited on Cu-substrates using the EPD method.…”
Section: Introductionmentioning
confidence: 99%
“…According to Equation (1), µ increases with increasing dielectric constant and zeta potential values, whereas it decreases for high viscosity values. It is imperative to optimize all the factors involved in the process to produce high-quality films or coatings [49]. These factors are discussed one by one.…”
Section: Key Parameters Affecting Epdmentioning
confidence: 99%