“…ATR-FTIR spectra confirmed the formation of PDA coatings and the presence of the expected chemical functionalities on the surface of the mesh samples (Figure 3 and Figure S3). All the mesh samples exhibited peaks associated with PP such as 2,916 cm −1 (C–H bands), 1,457 cm −1 (–CH 2 ), and 1,379 cm −1 (–CH 3 ) (Krylova and Dukštienė, 2013). Spectra of all the PDA-coated meshes contained additional peaks at 1,509 cm −1 (C = N of indole amine), 1,602 cm −1 (C=C of benzene ring), 1,723 cm −1 (C=O of quinone), and 3,100–3,700 cm −1 (N–H and O–H stretch vibration) (Patel et al, 2018).…”