“…[71] In the case of the refractory materials, as for example HfB 2 , the simultaneous synthesis and sintering produced dense ceramics (with 98% of the theoretical density) at lower pressure and temperature. [72] In order to explore the possibility of using SPS as a technique to can carry out a new sort of solid-state chemistry, the behaviour of the system M/V 2 O 5 (M ¼ Ag, Cu, Zn) during the SPS process has been investigated. The formation of different M x V 2 O 5 phases has been observed in a few minutes, even without a holding time at the final sintering conditions (Fig.…”