The molten salt synthesis has been known as an eco-friendly synthesis method because it does not produce hazardous waste and also, there is no requirement for a high calcination temperature. In this research, we synthesized SrBi 4 Ti 3.95 Fe 0.05 O 15 photocatalytic material via the molten salt method using NaCl, KCl, and NaCl/KCl salt. The diffractogram sample showed that SrBi 4 Ti 3.95 Fe 0.05 O 15 product obtained using KCl salt had successfully obtained with no impurities, but the SrBi 4 Ti 3.95 Fe 0.05 O 15 product synthesized using NaCl salt has found an impurities phase of Bi 4 Ti 3 O 12 and TiO 2 (brookite). SrCO 3 impurities was also found on SrBi 4 Ti 3.95 Fe 0.05 O 15 product that was synthesized using NaCl/KCl salt. The micrographs showed that the sample's morphology is plate-like and still found agglomeration. The results of the Kubelka-Munk calculation showed that the SrBi 4 Ti 3.95 Fe 0.05 O 15 has a band gap energy of about 2.32-2.55 eV.