2018
DOI: 10.1016/j.ceramint.2017.10.161
|View full text |Cite
|
Sign up to set email alerts
|

Synthesis and corrosion resistance of SiO2-TiO2-ZrO2-Bi2O3 coatings spin-coated on Ti6Al4V alloy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

1
3
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 18 publications
(4 citation statements)
references
References 24 publications
1
3
0
Order By: Relevance
“…In Figure 2(b) and Figure 2(c) respectively, the behavior of the difference between simple-laye rand two-layer coatings is not as visually significant as shown in Figure 1; however, it can be seen that a greater layer thickness allows a decrease in the corrosion rate of the material; a situation that confirms the trend that has been shown in terms of improvement in the anticorrosion response. This behaviour is in line with studies that have demonstrated efficient corrosion protection mechanisms with coatings [10][11][12].…”
Section: Resultssupporting
confidence: 91%
“…In Figure 2(b) and Figure 2(c) respectively, the behavior of the difference between simple-laye rand two-layer coatings is not as visually significant as shown in Figure 1; however, it can be seen that a greater layer thickness allows a decrease in the corrosion rate of the material; a situation that confirms the trend that has been shown in terms of improvement in the anticorrosion response. This behaviour is in line with studies that have demonstrated efficient corrosion protection mechanisms with coatings [10][11][12].…”
Section: Resultssupporting
confidence: 91%
“…In general, as the spin speed increases, the pellets are more homogeneous 18 . The grain size distributions for the coatings were also determined.…”
Section: Resultsmentioning
confidence: 99%
“…In this same graph the morphology of the oxides (white zones) can be appreciated, its size varies according to the speed with which the coatings were formed, that is to say, for speeds of obtaining 4000 rpm (Figure-1c) Greater agglomeration of the oxide with a smaller size of them. This can be attributed to the centrifugation process and consequently to the final thickness of the coatings, and also according to the investigations of Rajabi-Zamani and Feng the agglomerated structures observed in micrographs of Figure-1 are due to the aging or gelation time of the soles from which the coatings were formed 18,19,20 . Through the results of dispersive energies (EDX) it is possible to determine the composition of the oxides.…”
Section: Detection Methodsmentioning
confidence: 99%
“…Self-healing characteristics of SiO 2 resolve the microcracks of damaged sites and improve the material corrosion resistance, thermal stability and chemical resistance. 34,35 Silica stimulates the osteoblast cells to generate new bone formation, while its absence causes the anomalous growth of bone. The inclusion of silica ions in the coating can regulate calciumphosphorus in bone tissues and exhibit antibacterial effects.…”
Section: Introductionmentioning
confidence: 99%