Renewable natural resources such as eugenol, furfurylamine, stearylamine, and jute fiber were used to prepare polybenzoxazine composites. The purity of eugenol which is extracted from clove was confirmed by gas chromatography. FTIR, 1H, and 13C NMR spectroscopic analysis were used to determine the structure of eugenol and the benzoxazine monomers namely 6‐allyl‐3‐furfuryl‐8‐methoxy‐3,4‐dihydro‐2H‐1,3‐benzoxazine (EF‐Bz) and 6‐allyl‐3‐octadecyl‐8‐methoxy‐3,4 dihydro‐2H‐1,3‐benzoxazine (ES‐Bz) synthesized from it. The curing analysis from differential scanning calorimetric analysis shows that the onset of curing is shifted to lower temperature (161°C) for EF‐Bz, when compared with ES‐Bz (174°C). The thermal stability analyzed from thermogravimetric analysis shows that the polybenzoxazine EF‐Pbz has higher thermal stability (T5% = 361°C) with that of ES‐Pbz (T5% = 313°C). The storage modulus, tensile, and flexural strength of the EF‐Bz/Jute fiber composite show high value when compared with ES‐Bz/Jute fiber composites. POLYM. COMPOS., 37:1821–1829, 2016. © 2014 Society of Plastics Engineers