Synthesis of Cr2AlB2 MAB phase via Spark Plasma Sintering: Effect of temperature, dwell time, and Al content

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 7 publications
(1 citation statement)
references
References 26 publications
0
1
0
Order By: Relevance
“…However, the bending strength of WC-10HEA is only half of that of WC-10Co, with the value of about 1350 MPa. According to the above analysis, the relative density is the lowest and the size of WC particle is the largest, both of which are harmful to the bending strength of WC-10HEA [42]. In addition, the poor wettability may also be an important reason, considering that the pulling out of WC particles is the main fracture mode.…”
Section: Mechanical Propertiesmentioning
confidence: 97%
“…However, the bending strength of WC-10HEA is only half of that of WC-10Co, with the value of about 1350 MPa. According to the above analysis, the relative density is the lowest and the size of WC particle is the largest, both of which are harmful to the bending strength of WC-10HEA [42]. In addition, the poor wettability may also be an important reason, considering that the pulling out of WC particles is the main fracture mode.…”
Section: Mechanical Propertiesmentioning
confidence: 97%