“…During this CVD-like process, 41 the oblate sphere-shaped PVP-K30 (Figure S2a,b) located near the inlet vaporized and acted as a pore-forming agent. 42 Concurrently, the irregular rod-shaped MP (Figure S2c,d) near the air outlet acted as a morphology template, contributing as a source of C, O, N, and P for the synthesis of COPN-X materials (for detailed synthesis procedures for COPN-X, see Supporting Information: Synthesis of COPN-X). Reference samples labeled as MP-X were prepared without the use of PVP-K30 at various temperatures (400 to 800 °C) during the pyrolysis process (for a detailed synthesis procedure, see Supporting Information, synthesis of MP-X).…”