2006
DOI: 10.1016/j.ijimpeng.2004.09.008
|View full text |Cite
|
Sign up to set email alerts
|

Taylor impact of polyether ether ketone

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
15
0

Year Published

2007
2007
2024
2024

Publication Types

Select...
4
2
2

Relationship

0
8

Authors

Journals

citations
Cited by 33 publications
(17 citation statements)
references
References 16 publications
2
15
0
Order By: Relevance
“…The complex loading in compression of the Taylor test, where stress, strain rate, and final strain vary within the specimen makes it an ideal test for validating constitutive models, where the complex loading is thought to provide a more robust test of the model [36]. In polymers, the test has been used to understand the behavior of the materials under complex loading for modeling efforts [108][109][110][111][112][113] and to elucidate phase transitions in the polymeric materials [12,114].…”
Section: Dynamic Loading: Taylor Tests and Dynamic Tensile Extrusionmentioning
confidence: 99%
“…The complex loading in compression of the Taylor test, where stress, strain rate, and final strain vary within the specimen makes it an ideal test for validating constitutive models, where the complex loading is thought to provide a more robust test of the model [36]. In polymers, the test has been used to understand the behavior of the materials under complex loading for modeling efforts [108][109][110][111][112][113] and to elucidate phase transitions in the polymeric materials [12,114].…”
Section: Dynamic Loading: Taylor Tests and Dynamic Tensile Extrusionmentioning
confidence: 99%
“…Hutchings (1979) proposed an alternate one-dimensional elastic-plastic wave propagation analysis to calculate the yield stress in polymers and compared it with Taylor's analysis using experimental data on polycarbonate. Millet et al (2006) studied the behavior and failure initiation of poly(ether ether ketone) (PEEK) at velocities in the range of 150-400 m s À1 using high-speed photography. Rae et al (2004) studied the high temperature behavior of poly(tetrafluoroethylene) (PTFE).…”
Section: Introductionmentioning
confidence: 99%
“…It was also suggested that both PP and PS showed evidence of increased crystallinity due to shock loading. Such a response has been observed in polyether etherketone (PEEK), where Millett et al [21] showed a pronounced discolouration immediately behind the impact face during…”
Section: Introductionmentioning